Matbench v0.
More »
1 test dataset for predicting experimental band gap from composition alone. Retrieved from Zhuo et al. supplementary information. Deduplicated according to composition, removing compositions with reported band gaps spanning more than a 0.1eV range; remaining compositions were assigned values based on the closest experimental value to the mean experimental value for that composition among all reports. If you are viewing this on MPContribs-ML interactively, please ensure the order of theidentifiers is sequential (mb-expt_gap-0001, mb-expt_gap-0002, etc.) before benchmarking.
Other Info
columns |
| ||||
---|---|---|---|---|---|
entries | 4604 |